BALINIT® HARDLUBE High performance with minimal lubrication
Coating Properties
Coating Material
TiAlN + WC/C (a-C:H:W)
Microhardness* (HV 0.05)
3,000
Friction coefficient* against steel (dry)
0.15 - 0.20
Max. service temperature (°C)
800
Coating colour
dark grey
* depends on application and test conditions
BALINIT® HARDLUBE: the high hardness and temperature resistance of the TiAlN coating provide effective wear protection for cutting edges while the outstanding frictional and lubrication properties of the WC/C coating allow a smooth chips flow. The result: higher manufacturing reliability thanks to consistent and reproducible behaviour.Recommended applications:
tapping and drilling in materials that are hard to machine and form long chips
MQL (minimum quantity lubrication) or dry machining